  • For the specification of galvanized wire, the galvanized wire produced by our factory can range from No.8 to No.22, which refers to the BWG standard, that is, from about 4mm to 0.7mm, which can basically cover the type required by the customer. As for the raw material of galvanized wire, normally, we use Q195 mild steel, and some factories will also use SAE1006 or SAE1008. The following is the zinc coating, for galvanized wire, this is very important, the general zinc coating is about 50g/m2 to 80g/m2, some customers need high zinc galvanized wire, zinc coating can reach 200g/m2 to 360g/m2. The tensile strength of galvanized wire is usually 350n/m2 to 800n/m2. Then there is the packaging specification of galvanized wire. The specifications of small rolls of galvanized wire are 50kg/ roll, 100kg/ roll and 200kg/ roll. Of course, there are large rolls of galvanized wire, the weight can reach 300kg/ roll or 800kg/ roll.

  • Large roll galvanized wire phosphating film is dark gray to black gray, the thickness is generally 5-20μm, has better corrosion resistance in the atmosphere. Membrane is a microporous structure, strong adsorption ability to paint, such as used as paint bottom, corrosion resistance can be further advanced. Metal oxidation treatment: Add steel products to NaOH and NaNO2 mixed solution, heating treatment, the surface can form a layer of thickness of about 0.5-1.5μm blue oxide film, in order to reach the purpose of steel corrosion prevention, this process is called blue treatment, referred to as blue.

  • It was designed not only to be easy to install, but also to allow for quick and easy installation in harsh terrain such as cliffs, with little anchorage and little excavation. Based on the characteristics of heavy hexagonal mesh duplex structure, it can withstand the impact of falling rocks even when the steel wire is damaged.

  • Galvanizing can be done by zincate galvanizing or chloride galvanizing. Appropriate additives should be used to obtain a coating that meets the requirements of this standard. Light treatment should be carried out after light plating. The parts that need to be dehydrogenated for passivation should be passivated after dehydrogenation. Before passivation, 1%H2SO4 or 1% hydrochloric acid should be applied for activation for 5~15s. Passivation shall be treated with colored chromate unless otherwise specified in the design drawings.
  • The utility of the hexagonal net in the playground is very superficial, in each city to build the playground, are less than the shadow of the hexagonal net. In the stadium around the installation of hexagonal nets, not only can improve the stadium group image, but also convenient city residents to carry out a row of activities. Because the size of the plane or the surface of the object in the urban area is relatively small, many stadiums are built in the more prosperous and lively section, with the hexagonal net as a protective barrier, so it greatly reduces the spherical three-dimensional fly out of the field so as to affect the traffic order of bad things.

  • Nemator roller cage is connected by nemator connecting clasp with longitudinal tension bar fixed on the support, and the connection between longitudinal tension bar and support is selected. The 2.5mm cold-drawn galvanized steel wire is wound 2 times and then tightened and fixed. The bracket is set on the column and the cross side of the protective fence with a span of 3m. Other spans are only set on the upper part of the column, and the bracket and the protective fence are connected with the bracket hoop.

  • Zinc is a silver-white metal, brittle at room temperature, soluble in acid can also be soluble in alkali, known as amphoteric metal. Pure zinc in dry air is more stable, in humid air or containing carbon dioxide and oxygen water is small, the surface will generate a layer of basic zinc carbonate based thin film layer, it can delay the corrosion rate of zinc layer. The corrosion resistance of zinc coating in aqueous solution of acid, alkali and sodium chloride is stronger.

  • metal

  • Galvanized iron wire is divided into hot-dip galvanized wire and cold galvanized wire, using low carbon steel wire processing, after drawing forming, pickling rust removal, high temperature annealing, hot-dip galvanized, cooling and other processes. With good toughness and elasticity, the amount of zinc can reach 300 grams/square meter. It has the characteristics of thick galvanized layer and strong corrosion resistance. Galvanized iron wire can cut off the tie wire used in the building, the length is 20cm 30cm 40cm, can be cut off according to the requirements.

  • At the time of production, the annealing wire will be processed according to the performance of the material. According to different needs, the degree of hardness and softness can be changed, which can make it have more advantages, reduce the consumption of metal and reduce the cost of production. In the use of the time does not need to carry out daily maintenance and maintenance, not only can save a lot of time, but also can reduce the cost, but also has good stability, strong corrosion resistance, greatly extend the service life.

  • Before wall plastering, the wall column is connected to the gap construction wire mesh, which can play a certain strengthening and heat preservation effect. The mesh is hung on the interface surface of different grassroots, and the length of each side should meet the requirements of 100mm, so as to prevent shrinkage and cracking caused by different grassroots. Mesh wire diameter can also determine the effect and efficiency of construction, mesh fine laid up convenient soft, high construction efficiency; Of national standard can assure quality, but laid respect is inferior to fine construction fast.

  • Wire flexibility and elongation is good, can withstand the pressure of mechanical operation, in our country’s industry has played a very important role. There are many kinds of iron wire, the most common is to give black iron wire, galvanized iron wire. The corrosion resistance of the outer coating is effectively improved, but the phenomenon of crevice corrosion will be found after long-term use.


  • Post time: 24-10-22
  • Factors affecting the corrosion resistance of galvanized wire: The corrosion resistance of galvanized wire is affected by many factors, mainly including the following aspects.

  • Post-plating treatment (passivation, hot melting, sealing and hydrogen removal, etc.) for the purpose of enhancing protective properties, decoration and other special purposes. After galvanized, chromate passivation or other conversion treatment is generally required to form the corresponding type of conversion film, which is one of the key processes to ensure the quality of post-plating.

  • Post time: 20-12-22
  • The service condition and service life of galvanized iron wire or components are closely related to the thickness of the coating. The more strict the use conditions and the longer the service life, the thicker the required layer of galvanized iron wire should be. Different products, according to the specific environment (temperature, humidity, rainfall, atmospheric composition, etc.) to determine the expected service life of the coating thickness, blind thickening will cause all kinds of waste. But if the thickness is insufficient, it will not reach the expected service life requirements. Different manufacturers, according to their own equipment conditions, in the case of determining the plating, the first preparation of a more complete and reasonable process flow, clear plating parameters, control plating solution concentration, standard operation.


  • Post time: 09-05-23
  • At present, there are two main kinds of electric galvanized wire products, hot dip galvanized wire and electric galvanized wire. The difference is that the way of galvanizing is different, and the quality of the products is different. Hot dip galvanized wire zinc layer thick, corrosion resistance is stronger, but correspondingly, the price is high. Galvanized wire zinc coating thin, corrosion resistance is poor, but the price is low.

  • Packaging is also very important, cut wire to do a good job in the bundle with plastic film tightly packed, and then in the regular box, to fill the whole box is very full and sealed, it is best not to have a half box of conditions, if there is a half box to fill with foam and other things, so that in the transit cut wire will not receive a little damage.

  • (8) galvanized wire coated hexagonal mesh is coated with a layer of PVC protective layer on the surface of galvanized iron wire, and then woven into a variety of specifications of hexagonal mesh. This layer of PVC protective layer will greatly increase the service life of the net, and through the choice of different colors, so that it can be integrated with the surrounding natural environment.